Details:
Dyeing with the same specification (210D/12 strands) nylon, one by steam shaping, one by natural setting, using steam as the line is thicker (fixing temperature is 80 degrees for 15 minutes, evacuating 3 times), the result is using steam shaping The dyed out color is not uniform. Natural stereotypes do not produce such phenomena.
solve:
Steam setting: Due to the large humidity, the dye at 80 degrees of water vapor, acid dyes, water-soluble dyes, migration is serious, there will be color phenomenon, it is recommended to change the hot air stereotypes, or to prevent the migration agent, the first pre-baking.
Another: drum dyeing uneven phenomenon:
1, first of all have to look at whether it is a problem of drying, the method is simple: after dyeing the cylinder carefully, the yarn can be cut to see if the dyeing itself is not uniform, if it is uneven dyeing, can strengthen the pre-processing and dyeing plus Penetrants promote staining!
2. If it is a problem that occurs during drying, it is recommended to use anti-migration agent.
For more content, please follow this site
Polyester Disperse Print Fabric
Polyester Disperse Print Fabric,Polyester Microfiber Disperse Printed Fabric,Disperse Printed Bed Sheet Fabric,Disperse Bed Sheet Polyester Printed Fabric
Shaoxing City Shengfeng Import And Export Co.,Ltd. , https://www.sunfeelfabric.com